Technical Specifications
Applicable in the indoor hot and cold water pipe systems, Fırat Composite Pipe and Fittings are produced according the UBM-05-BK-056 quality criteria published by Turkish Standards Institute.
Property |
Value |
Test Parameters
|
Test Method |
Dimensional Stability |
%2 |
Test Temperature (Cº) |
135 |
Test Duration (hº) For e> 8 mm |
1 |
8 mm < e < 16 mm |
2 |
For e> 16 mm |
4 |
Test Sample |
3 |
|
EN 743 |
Falling Ball Test Impact Resistance |
No breaking, cracking |
Test Temperature (Cº) |
0 |
Test Sample |
10 |
Height (cm) |
50 |
Test Mass (gram) |
|
For dn 20 mm; |
250 |
For dn 25 mm; |
500 |
For dn 32 mm; |
800 |
For dn 40 mm; |
1,250 |
For dn 50 mm; |
2,000 |
For dn 63 mm; |
3,200 |
For dn 75 mm; |
10,000 |
For dn >90 mm; |
16,000 |
|
|
Melting Mass Flow Rate (Raw Material) |
<0.5 gram / 10 minutes |
Test Duration (hº ) |
230 |
Mass (kg) |
2,16 |
Test Sample |
3 |
|
ISO 1133 |
Melting Mass Flow Rate (Pipe) |
When raw material result is compared, difference must be max 30%. |
Test Duration (hº ) |
230 |
Mass (kg) |
2,16 |
Test Sample |
3 |
|
ISO 1133 |
Property |
Value |
Test Parameters |
Test Method |
Internal Pressure Resistance |
No damage during test duration |
Hydrostatic (circle) Tension (Mpa) |
Test Temperature (°C) |
Test Duration (h) |
Test Sample Number |
16,0 |
20 |
1 |
3 |
4,3 |
95 |
22 |
3 |
3,8 |
95 |
165 |
3 |
3,5 |
95 |
1000 |
3 |
|
TS EN ISO 1167 - 1/2 |
Fırat Composite Pipes are certified by TSEK and GOST institutions as they do not pose any harmful effect on human health and do not change the color, smell and taste of the water. The Turkish Food Codex compliance of Fırat Composite Pipes is certified by Sanitation Institute.